Hello Everyone,

Basically, I've had a go at running before I can walk and stumbled into a problem or 2 I'm hoping somebody can help me with.

The first mould I've had a go at making is for a roll top bath which wasn't going too bad until I had to use Reface to fix any high and low points.
I had never used a spray gun before and didn't do any practice pieces beforehand, I just made sure the gun sprayed properly and jumped in and went for it.

The gun worked okay briefly and then I started having problems with intermittent spraying and no matter what I done, I couldn't get it working properly.
After trying various things the gun seized and was ruined. My fix for this was to brush it on and in my naivety I didn't think it would be too bad... :/

I've gone upto a 40 grit paper and leveled out the brush marks/high points pretty well but, now I have low points where wood is showing through (only a couple of places and nothing too major) and high points where it's still pretty thick Reface (in the corners and where the base meets the walls of the tub) and obviously the scratches from the 40 grit paper..

What I'd like help with is, how is it best to save my hard work, does anybody have any pointers/do's/don'ts before I destroy things further? Should I sand things down and use a paint roller to put on another coat of Reface and start again to a certain extent?

I was thinking to carry on sanding down with finer grit paper, go over any bare bits with more reface (and there maybe a couple of bits that could do with a thin layer of filler first?), and blend it all in with some fine grit paper..

What does anybody think? Any help/ideas are greatly appreciated.. And yes, I know I've been a bit of an impatient arse about all this and I will organise a spray painting course as soon as money permits!

Thanks for your're time reading this, I hope you can help. Rob

Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You need to choose a pigment suitable for your resin system.  The pigment you linked to is a silicone pigment.

You can fill in the low areas, but if it is easy to sand, then coat the whole part as you don't know how low some of the areas are.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
robenergy
robenergy
Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)
Group: Forum Members
Posts: 20, Visits: 216
Warren (Staff) - 1/8/2018 11:49:36 AM
You need to choose a pigment suitable for your resin system.  The pigment you linked to is a silicone pigment.

You can fill in the low areas, but if it is easy to sand, then coat the whole part as you don't know how low some of the areas are.


The Reface I used is a polyester based filler.

This particular filler is quite hardwork to sand down. I do feel reasonably happy about just patch filling the bear areas and then blending it all together. But, obviously I want a really good finish, so how bigger corner am I cutting by only spot filling and blending in.. would it still give me acceptable results??

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
robenergy - 7 Years Ago
Warren (Staff) - 7 Years Ago
robenergy - 7 Years Ago
Warren (Staff) - 7 Years Ago
robenergy - 7 Years Ago
Hanaldo - 7 Years Ago
robenergy - 7 Years Ago
Hanaldo - 7 Years Ago
robenergy - 7 Years Ago
Hanaldo - 7 Years Ago
robenergy - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search