Hello Everyone,

Basically, I've had a go at running before I can walk and stumbled into a problem or 2 I'm hoping somebody can help me with.

The first mould I've had a go at making is for a roll top bath which wasn't going too bad until I had to use Reface to fix any high and low points.
I had never used a spray gun before and didn't do any practice pieces beforehand, I just made sure the gun sprayed properly and jumped in and went for it.

The gun worked okay briefly and then I started having problems with intermittent spraying and no matter what I done, I couldn't get it working properly.
After trying various things the gun seized and was ruined. My fix for this was to brush it on and in my naivety I didn't think it would be too bad... :/

I've gone upto a 40 grit paper and leveled out the brush marks/high points pretty well but, now I have low points where wood is showing through (only a couple of places and nothing too major) and high points where it's still pretty thick Reface (in the corners and where the base meets the walls of the tub) and obviously the scratches from the 40 grit paper..

What I'd like help with is, how is it best to save my hard work, does anybody have any pointers/do's/don'ts before I destroy things further? Should I sand things down and use a paint roller to put on another coat of Reface and start again to a certain extent?

I was thinking to carry on sanding down with finer grit paper, go over any bare bits with more reface (and there maybe a couple of bits that could do with a thin layer of filler first?), and blend it all in with some fine grit paper..

What does anybody think? Any help/ideas are greatly appreciated.. And yes, I know I've been a bit of an impatient arse about all this and I will organise a spray painting course as soon as money permits!

Thanks for your're time reading this, I hope you can help. Rob

Reply
robenergy
robenergy
Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)Supreme Being (185 reputation)
Group: Forum Members
Posts: 20, Visits: 216
Warren (Staff) - 1/8/2018 9:34:03 AM
If you have gone down to the wood, you need another layer really to ensure you get a good finish.  What you can do is pigment the new layer a slightly different colour to the layer underneath.  That way as you sand, you can see how deep you are cutting.


Hi Warren, thanks for the reply.

So what you think, I need to apply a coat of  reface to the whole mould or just the bear patches and blend it all together?

Nice idea about the pigment,, would something like this be good to use?- https://www.ebay.com.au/itm/Latex-Colourant-RED-2oz/322336081407?hash=item4b0cba45ff:g:ywcAAOSw3utY4Wqh

Edited 7 Years Ago by robenergy
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
robenergy - 7 Years Ago
Warren (Staff) - 7 Years Ago
robenergy - 7 Years Ago
Warren (Staff) - 7 Years Ago
robenergy - 7 Years Ago
Hanaldo - 7 Years Ago
robenergy - 7 Years Ago
Hanaldo - 7 Years Ago
robenergy - 7 Years Ago
Hanaldo - 7 Years Ago
robenergy - 7 Years Ago