Jadleybray
Jadleybray
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 85
Super newbie to cf, been reading alot on properties and processes. Lets talk tooling, specifically router process as I do not have a CNC yet. Parts I'd like to make are fairly simple and I have aluminum patterns to follow. So I have two routers with up to 16,000 rpms available to use, and already purchased a couple of carbide bits, one 1/4" shank other 1/8" shank. I looked for days for a flush cut bit with a roller bearing thinking it would be ideal for using a pattern, however did not find one. So I went with this bit
https://www.toolstoday.com/solid-carbide-carbon-graphite-and-carbon-fiber-panel-cutting-router-bits.html?variantids=12012,0&keywords=46264
In hindsight I see it is not recommended for handheld routers, however on a couple of test passes using a straight edge cutting a 6.5mm cf plate worked well. I am concerned about digging into the pattern as the depth of the cutter has to be set precisely. Any suggestions here? Ideally a bit with a bearing would be the ticket, any one seen a full carbide bit like this?
Speed....from what I've read, and the short test piece, looks like high rpm's is the ticket for a smooth edge needing minimal work to finish. Any input is appreciated.
Reply
Like
7
Reply
Jadleybray
Jadleybray
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 10,
Visits: 85
Got to start somewhere, figured I'd mess with some basic shapes before buying software.
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Router cutting cf from template
Jadleybray
-
8 Years Ago
For cutting most carbon sheet we tend to go with PCB cutting bits. They cut cleanly and precisely. They will blunt after a reasonable amount of time but the cost is low enough for them to be...
Warren (Staff)
-
8 Years Ago
Got to start somewhere, figured I'd mess with some basic shapes before buying software.
Jadleybray
-
8 Years Ago
Let us know how you get on!
Warren (Staff)
-
8 Years Ago
Well I was never one to cheap out on tools, and found a diamond carbide impregnated 1/4 flush but with guide bearing. Routered out a few items recently with good results. Quick finish on the belt.....
Jadleybray
-
8 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search