CNC Machining and Finishing Epoxy Tooling Board to Produce and Accurate Composites Pattern


CNC Machining and Finishing Epoxy Tooling Board to Produce and Accurate Composites Pattern
Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Everyone,

Hopefully a few of you have noticed that we've been publishing a number of new video tutorials recently. I've now published the first two (out of three) of a new series which shows the end-to-end process for starting from a CAD design, CNC machining the pattern from epoxy block then sealing and preparing the pattern before taking a prepreg carbon fibre mould off the pattern. In the next video (not done yet) we'll finish off by using the prepreg mould to produce a carbon fibre part.

Essentially, in this series what we're trying to demonstrate is the 'other way' to make composite parts, using technology and high tech materials to replace the more manual traditional methods. This is a topic that comes up every time during our training courses and so hopefully this is a process (and tutorial series) that people will find interesting (and maybe useful). The price of perfectly usable CNC equipment is coming down all the time and the quality and availability of 3D CAD systems (like Fusion360) is moving the baseline of what is achievable at home or in a small workshop or business. Our new products and tutorials aim to support this revolution. Also, in this current climate where people are very focused on the idea that 3D printers are the answer to everything, hopefully we can steer a few people towards the understanding that for most composites processes a CNC router is a far more suitable piece of kit to invest in.

So, this first tutorial in the series we demonstrate how to CNC machine epoxy tooling board and then seal and finish it using epoxy board sealer.


I'd be very happy to discuss any of the topics raised in the videos including how these processes and materials might be used in your projects.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 8 Years Ago by Matt (Staff)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh, a good point.

Ive been speaking to a friend of mine today who built his own CNC router with Chinese framework and American/German electronics. He uses it for cutting 10mm aluminium, mostly 2D/2.5D stuff but says he is sure it would do what I'm wanting it to do with ease. Extremely little backlash, doesnt get any chatter or lost steps so long as he keeps to 0.2mm passes and doesnt get impatient with the feeds, and he says it is accurate to 0.1mm as long as everything stays in tune.

So I may go have a play with it sometime, see if we can test it's limitations. He is also currently planning on building a new one, so I may share that build with him and see if we can build something that suits the both of us.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matt (Staff) - 8 Years Ago
Premium Composites - 8 Years Ago
Matt (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
rmaddock - 8 Years Ago
Matt (Staff) - 8 Years Ago
Sebasan - 7 Years Ago
Premium Composites - 8 Years Ago
Matt (Staff) - 8 Years Ago
Theaumoix - 8 Years Ago
cumberdale - 7 Years Ago
Matt (Staff) - 7 Years Ago
cumberdale - 7 Years Ago
Matt (Staff) - 7 Years Ago
CaveDweller - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
cumberdale - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
scottracing - 7 Years Ago
Sebasan - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search