CNC Machining and Finishing Epoxy Tooling Board to Produce and Accurate Composites Pattern


CNC Machining and Finishing Epoxy Tooling Board to Produce and Accurate Composites Pattern
Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Everyone,

Hopefully a few of you have noticed that we've been publishing a number of new video tutorials recently. I've now published the first two (out of three) of a new series which shows the end-to-end process for starting from a CAD design, CNC machining the pattern from epoxy block then sealing and preparing the pattern before taking a prepreg carbon fibre mould off the pattern. In the next video (not done yet) we'll finish off by using the prepreg mould to produce a carbon fibre part.

Essentially, in this series what we're trying to demonstrate is the 'other way' to make composite parts, using technology and high tech materials to replace the more manual traditional methods. This is a topic that comes up every time during our training courses and so hopefully this is a process (and tutorial series) that people will find interesting (and maybe useful). The price of perfectly usable CNC equipment is coming down all the time and the quality and availability of 3D CAD systems (like Fusion360) is moving the baseline of what is achievable at home or in a small workshop or business. Our new products and tutorials aim to support this revolution. Also, in this current climate where people are very focused on the idea that 3D printers are the answer to everything, hopefully we can steer a few people towards the understanding that for most composites processes a CNC router is a far more suitable piece of kit to invest in.

So, this first tutorial in the series we demonstrate how to CNC machine epoxy tooling board and then seal and finish it using epoxy board sealer.


I'd be very happy to discuss any of the topics raised in the videos including how these processes and materials might be used in your projects.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 8 Years Ago by Matt (Staff)
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Anders Ryberg - 11/28/2017 12:52:03 PM
Hi,

Great tutorials, very interesting for a project I am working on. However, my pattern is already produced using PU600 and not EP700, finished off with 2K car paint. Will this work with the XPREG Tooling Prepreg?


Best Regards,
Anders

Mmmm, good question. The problem with PU modelboard is that PU inhibits the cure of epoxy at elevated temperatures. Having said that, you've covered your PU board with 2k car paint (which will be either acrylic or could be PU itself) and therefore the tooling prepreg would not be in contact with the PU board so you might be OK.

I'd say the first thing to look into is what your 2k car paint is made from. If the paint itself is polyurethane then you might still have the same problem. If the paint is acrylic then it might be OK but I think I would have to suggest a trial to see if the paint itself inhibits the cure at all. Because the initial cure is done at a pretty low temperature (which should just about be OK for the paint) there is a good chance that the cure inhibition won't occur but it really will come down to the individual behaviour of that paint system.


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matt (Staff) - 8 Years Ago
Premium Composites - 8 Years Ago
Matt (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
rmaddock - 8 Years Ago
Matt (Staff) - 8 Years Ago
Sebasan - 7 Years Ago
Premium Composites - 8 Years Ago
Matt (Staff) - 8 Years Ago
Theaumoix - 8 Years Ago
cumberdale - 7 Years Ago
Matt (Staff) - 7 Years Ago
cumberdale - 7 Years Ago
Matt (Staff) - 7 Years Ago
CaveDweller - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
cumberdale - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
scottracing - 7 Years Ago
Sebasan - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search