			            I am not aware of any products that can be applied to GC50 to make it tacky again.  Spray tacks or similar materials are a popular choice although we would not recommend using it on top of GC50 unless absolutely necessary as any excess build up will be visible through the gelcoat and impossible to rectify.                   
			            
  				