I see you say the shelf life is around 4 month's for the uni mould stuff is this an absolute? I bought a 25kg tub of uni mould tooling resin last year but didn't get round to using it, will this now be no good? 
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I would recommend that you do a small test of the resin to see if and how it cures. The Uni-Mould products do have the shortest shelf life of any of our products - in part due to the high proportion of fillers in the gel coat and the special formulation.  The Tooling Resin is not quite as sensitive.  However, do a good test before you make a decision on using it or not.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search