Rocket Airframe


Author
Message
ROCKET COL
ROCKET COL
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 4, Visits: 16
Hi all, just putting this out to see what you all think.
Looking to coat a spiral wound cardboard tube 142mm OD with 2mm wall 2m tall.
it will just add more strength to the tube, it needs to be light yet strong.
It also needs to have a good finish, may or may not be painted.
What do I cover it with?
Sleeve, woven cloth, fibreglass, carbon, Kevlar????
Peelply or vac bagging?? the tube is hollow and needs to keep its shape as parts fit in and slide out to allow recovery.
There are also 3 large fins at the base, so do I do tube first, then cut slots and slide over fins then fillet the joints or do i do in 1 hit
and hope it looks ok.
Depending on motors it could be going up to 650mph in a few seconds to about 10,000 feet, also has to take landing on parachute.
I know a lot to take in just asking.
Thanks
Colin
Reply
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
if youve got a metal pipe/pvc pipe of almost the right outside diameter to fit in your card tube, then you could add that during moulding to temporarily strengthen the tube.