Visits: 1.9K
|
Back before I discovered infusion, i used to lay out a flat sheet of vacuum bagging film, then very lightly coat "the outside" of a cut to shape piece of CF and leave it to cure to a sort of "soft tacky state" .. Then you can drape/place the carbon fibre a bit like a piece of pre-preg in the mould, leave it a bit to cure to a slightly harder state of tack, then soak with resin, and add additional layers. The end product will have some slightly "dry" areas, so I always clear coated the parts. This technique can make it possible to make quite complex parts with "wet lay" only