Soric XF vs Soric SF


Author
Message
FLD
FLD
FLD
posted 8 Years Ago HOT
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Morning folks.  I've just bought some soric XF to have a play with.  It has larger cells than the SF variant so I was expecting it to be lighter overall but the resin channels are also larger so I expect it's not going to be any lighter.  Has anyone run a back to back comparison of the two looking at weight and part rigidity?  I'm curious to see what everyone else makes of it.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Will have to try harder to find the LRC in Aus, it sounds great. 