Parts get soft in the sun


Author
Message
Carbon Tuner
Carbon Tuner
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 104, Visits: 422
Hey ahhh, why these parts getting so soft in the sun?

 

How can I fix this? I do resin infusion, is it time to get a parts oven and switch to a higher temp tooling gel?



If Brute Force Isn''''t working your not using enough...
Reply
Carbon Tuner
Carbon Tuner
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 104, Visits: 422
K guys I am going to try and heat cure my mold,

I did read for the orange tooling gel I am using now I can go 150F. Then after 16 hrs of that I can go 190F the next time.

So now comes the time I need a parts oven...

I also have a part I may just attempt to heat cure out of the mold, as long as the part reaches 150 or so it will stiffen up or does it have to be in the heat for a certain amount of time



If Brute Force Isn''''t working your not using enough...
Edited 14 Years Ago by Carbon Tuner
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Carbon Tuner - 14 Years Ago
NikCFC - 14 Years Ago
             whats post cure?
Carbon Tuner - 14 Years Ago
SebRS - 14 Years Ago
NikCFC - 14 Years Ago
Bruce - 14 Years Ago
Matt (Staff) - 14 Years Ago
Bruce - 14 Years Ago
ebf2k - 13 Years Ago
Carbon Tuner - 14 Years Ago
Joe - 14 Years Ago
Warren - 14 Years Ago
twissta - 14 Years Ago
Warren - 14 Years Ago
Carbon Tuner - 14 Years Ago
Warren - 14 Years Ago
Ortonporton - 13 Years Ago
TomDesign - 13 Years Ago
NikCFC - 13 Years Ago
matthieutje65 - 13 Years Ago