Parts get soft in the sun


Author
Message
Carbon Tuner
Carbon Tuner
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 104, Visits: 422
Hey ahhh, why these parts getting so soft in the sun?

 

How can I fix this? I do resin infusion, is it time to get a parts oven and switch to a higher temp tooling gel?



If Brute Force Isn''''t working your not using enough...
Reply
Warren
Warren
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Administrators
Posts: 214, Visits: 783
I guess you could leave it a few weeks if you cant get the elevated temperatures.

if you cant stretch to an oven, you can use electric blankets.  The one i have heats to 40 degrees celcius which although not as good as 60 degrees, can still be better than just room temp.

Another way of doing a cheap oven if you have space is to use breeze blocks to make a basic oven shape, line it with insulating foam (the sealed foil covered stuff). then use a 2kw fan heater to heat the box up.  Only problem is they need careful temperature monitoring really.  You could probably buy some thermostat controlled heating element but i wouldnt want to leave such a thing unattended really if its not a proper oven.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Carbon Tuner - 14 Years Ago
NikCFC - 14 Years Ago
             whats post cure?
Carbon Tuner - 14 Years Ago
SebRS - 14 Years Ago
NikCFC - 14 Years Ago
Bruce - 14 Years Ago
Matt (Staff) - 14 Years Ago
Bruce - 14 Years Ago
ebf2k - 13 Years Ago
Carbon Tuner - 14 Years Ago
Joe - 14 Years Ago
Warren - 14 Years Ago
twissta - 14 Years Ago
Warren - 14 Years Ago
Carbon Tuner - 14 Years Ago
Warren - 14 Years Ago
Ortonporton - 13 Years Ago
TomDesign - 13 Years Ago
NikCFC - 13 Years Ago
matthieutje65 - 13 Years Ago