Group: Forum Members
Posts: 61,
Visits: 871
|
Hi,
First of all you have to check the tg (Glass Transition Temperature - The glass transition is the temperature where the polymer goes from a hard, glass like state to a rubber like state) of the epoxy you're using, the higher the better.
Post curing is actually curing in an oven / autoclave at higher temperatures raising the temperature little by little after initial curing has taken place while the part stays in the mold to avoid distortion.
|