Group: Forum Members
Posts: 22,
Visits: 116
|
Hi Warren,
I thought someone would have an answer, though I can understand some designers showing enough to demonstrate the innovation
in their work but still not showing enough for others to replicate. The carbon fibre tow seems to be used in just a single thickness with just the crossing wire mesh effect providing strength. It seems to me that the more crossings you have to stronger the finished article.Thank you for your prompt reply.
Trevor
|