Which adhesive is the best to attach Kevlar braid fabric to cured epoxy carbon fibre. I want to make a living hinge for an aileron on an uav plane.
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I would use a toughened epoxy glue or a methacrylate.