Group: Forum Members
Posts: 2,
Visits: 50
|
Thank you for the help. If I kept the 3 layers on both the top and bottom and put a single 7th layer of prepreg carbon fiber in the middle between the two sandwich panels (to give them both a surface to adhere to), then it shouldn't be significantly weaker than the first proposal, correct?
|