BigChief
BigChief
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 50
Let's say I was going to make a sandwich panel:
---3 layers of carbon fiber---
---1-inch nomex honeycomb---
---3 layers of carbon fiber---
What if I instead made:
---2 layers of carbon fiber---
---half-inch nomex honeycomb---
---2 layers of carbon fiber---
---half-inch nomex honeycomb---
---2 layers of carbon fiber---
Both sandwich panels total the same amount of material and weight... would the second option be as stiff/strong?
Are there any best practices on how many layers of carbon fiber to honeycomb would give the best strength-to-weight ratio? It would be nice to have a general idea without resorting to FEA tools.
Reply
Like
3
Reply
Fasta
Fasta
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Generally this is not any stronger.
Usually you can consider the middle of the sandwich as a neutral area where fibre layers would not be taking any loads.
The outer skins take all the loads of compression and tension while the core mostly just holds the skins apart.
In fact since your second proposal has just two layers on the outer skins then it would not be as strong as the first proposal that has three layers.
Fastacraft Facebook page
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Would a stacked honeycomb sandwich panel work?
BigChief
-
9 Years Ago
Generally this is not any stronger. Usually you can consider the middle of the sandwich as a...
Fasta
-
9 Years Ago
Thank you for the help. If I kept the 3 layers on both the top and bottom and put a single 7th layer...
BigChief
-
9 Years Ago
[quote][b]BigChief (30/11/2016)[/b][hr]Thank you for the help. If I kept the 3 layers on both the...
Fasta
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search