Kirk
|
|
Group: Forum Members
Posts: 6,
Visits: 205
|
Hi guys, I've been on here for a while, I originally looked into making a direct replacement dash centre console, but quickly came to realise the only option was to skin it. Any way, in the end, I got a company to do the centres for 3 cars for me so I could get pictures, get them up on my website and offer them for sale, these would have been done to order and I was promised they would take a week. So, with a week in mind, a customer let us borrow his dash to be sent off in the return that they get it for cost price. 2 months on, we are now only just looking at possibly getting the parts back, obviously this isn't a model I can run with for my business. They were going to have my entire car to do doors, roof, boot, etc etc, but on the current time scales, it'd prob take me a year to get it back. So, I am back at looking to do carbon myself. Anyway, on to my main point........ I am looking to clear the double garage out and skin my entire car, in fact, we are actually looking at doing 3 cars all in, which will all be demo cars for my tuning company. I would like to, once I have the hang of using carbon more, make the panels such as the roof, doors, boot, wings, bonnet, spoiler, mirrors etc completely from carbon in an OE style. Is the door, boot and bonnet possible to do matching OE style and use original locks, latches, door cards, windows etc? But, to start, I shall remove the windows from the car and skin it. I have worked out that I have approx 25sqm to cover on the car, so im looking at 25m2 of 200g 2x2 plus some mistakes and a couple of small practice pieces. How much resin would I need? I'm looking to do it by the 1st black layer of resin, lay carbon, coat of epoxy, 3x coats of epoxy (I am considering spraying this in my spray booth, would this work?), final coat of epoxy (again, looking to possibly spray), sand it all down, leave for a week, 3 coats of laquer, wet flat and another 3 coats of lacquer, wet flat 800, leave for 2-4 weeks, wet flat 1200, 2000, 2500 polish. Is there any advice, hint, tips etc etc that anyone can offer?
|
|
|
Fasta
|
|
Group: Forum Members
Posts: 468,
Visits: 3.5K
|
Ok then. Lets do it! I am sure there are plenty of techniques and tips and everyone will chip in with their 2c. This is what I would consider. Spray the car with black etch primer. I have some single pack stuff yet it is labeled as epoxy etch coat?? Abrade the etch coat and lay out your carbon. You can do it dry and wet through with the epoxy resin (surfboard style) which will help with getting the fibre to lay well and look right. I am sure you have seen others do a tack coat of epoxy too, I believe this is better for smaller and detail parts so the fabric can be stuck into details better and it stays. Downside is that it is harder to lay down straight and you likely can't just pull it back off without making a mess of the material. Another technique is to use a light mist of spray glue like 3M super 77 to hold the material in place and then wet through with your epoxy resin. Next, once the carbon has tacked off quite well but not fully cured float on a coat of a specific epoxy coating resin to help fill the weave. Let this coat fully cure. Sand back back the epoxy resin coat without sanding into the carbon too much. It can touch the carbon here and there but don't rub too far. Next coat is the Duratec Sunshield, this is like another filler coat but this stuff is far easier to sand than epoxies. You can go straight 180grit or 240grit. Then 600 and 800 wet sanding. Then the two part paint clear coats.
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
Hi fasta where do you buy the duratec sun shield from
|
|
|
Fasta
|
|
Group: Forum Members
Posts: 468,
Visits: 3.5K
|
In Australia I buy it from ATL composites in Queensland.
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
I am In Perth Australia to Is there any where local to us I have heard off people using 2 pack clear to build up and fill Or is it better to use the sun shield as u sayed in the description ? Thanks
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
I am In Perth Australia to Is there any where local to us I have heard off people using 2 pack clear to build up and fill Or is it better to use the sun shield as u sayed in the description ? Thanks
|
|
|
Fasta
|
|
Group: Forum Members
Posts: 468,
Visits: 3.5K
|
Coxo (06/01/2017)
I am In Perth Australia to Is there any where local to us I have heard off people using 2 pack clear to build up and fill Or is it better to use the sun shield as u sayed in the description ? Thanks The sunshield is far better and easier to fill than two pack clears. You can't buy it local.
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
Fasta would you just use sun sheld over this part now to build up ? Thanks
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
Hi fasta would you sell me a small amount for me to try it out
|
|
|
Fasta
|
|
Group: Forum Members
Posts: 468,
Visits: 3.5K
|
Coxo (09/01/2017)
Hi fasta would you sell me a small amount for me to try it out Pls Thanks Sure, drop in, U2, 4 Dobra Rd Yangebup.
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
Hi fasta will u be a your unit tomorrow And I'll pop in ? Cheers graham
|
|
|
Fasta
|
|
Group: Forum Members
Posts: 468,
Visits: 3.5K
|
I'll be there first thing in the morning hour or so from 9am. 40 deg C public holiday, too hot for work.
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
Cool see u at 9 am I forget it's a holiday
|
|
|
Coxo
|
|
Group: Forum Members
Posts: 39,
Visits: 476
|
That duratec tec sun sheid is great look at the finish Thanks fasta for giving me some to try How long dose it take to dry It still seams Tacky but hard if u no what I mean
|
|
|