Epoxy/Polyester Table Top with Wood


Author
Message
Matt
Matt
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Forum Members
Posts: 4, Visits: 43
I have a project I would like to attempt but not 100% on how to achieve it, any input would be appreciated.

I am looking to use a white epoxy or polyester to encapsulate some wooden branches to create an indoor table top. I will cut a flat surface onto the branches before laying them into an open mould. The branches will be visible on the table top but as the epoxy/polyester will be pigmented white you won't see any branches that aren't on the top surface. I hope that makes sense.

The upper surface needs to be durable, i.e. not easily scratched and fairly resistant to heat. It also has to be UV resistant - no discolouration.

Initially I was thinking of using Waterclear Polyester Casting Resin with a white pigment and treating the wood with Polyester Infusion Resin before pouring to reduce are bubbles.

My concern with this approach is the durability of the Waterclear Polyester as a table top.

Would it be possible to pour a very thin (1-2mm) layer of epoxy (with white pigment) in order to get the durable surface then make the bulk of the'body' in polyester (up to 50mm thick).

Is this possible?

Would the epoxy yellow over time?

Is there anyway I can use filler in the polyester pour to reduce costs?

Is there anything else I should consider?

TIA

Matt
Reply
Matt
Matt
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Forum Members
Posts: 4, Visits: 43
Thanks Hanaldo

I'll trial epoxy and polyester separately. I'm not convinced the polyester casting resin will be durable enough for a table top.

The plan is to pour a small amount of resin and place the wood into the thin layer which will hopefully fill all the gaps. I'll sand back the surface if its not perfect. I've also purchased a polyester infusion resin to treat the wood prior to casting.

I was planning on doing this in the garage but it sound like the exothermic reaction of polyester is very temperature sensitive and the garage will be too cold.