Group: Forum Members
Posts: 460,
Visits: 5.2K
|
it definitely looks like the material isn't wetted out properly or there's some excess resin being pushed out. Are you wetting out each ply individually then laying them on top of each other? I would add a cork dam or use some other means of retaining the resin into the laminate when you are pressing, also what temperature are you curing at?
|