General Composites Discussion
»
Cover 10mm carbon fiber tube inside evenly with epoxy resin?
Cover 10mm carbon fiber tube inside evenly with epoxy resin?
Post Reply
Like
7
Cover 10mm carbon fiber tube inside evenly with epoxy resin?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
valzine
valzine
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 21
Hello everyone,
I've been searching the forum but couldn't find the answer to my question. I'm trying to cover
the inside
of a 10mm carbon fiber tube with inner diameter of 8mm in thin layer of high temp food safe epoxy resin. The inner aperture is very important to me (precision I'm looking for is up to hundreds of mm). I achieve needed inner diameter by drilling with precise drill bits. The tube is approximately 50mm in length. My questions are:
1. Can I somehow spay the epoxy inside or do I have to apply it by hand? If applied by hand, what would be the best tool to use?
2. Would 3k rolled carbon fiber tube absorb the thin layer of epoxy resin and leave the inner aperture the same? Or do I have to polish it somehow (drill again?) after I apply it?
Here is the resin I'm intending to use:
https://www.atomadhesives.com/FDA-Grade-Food-Medical-Epoxy-Adhesives/AA-BOND-FDA8-FDA-Grade-Epoxy-Adhesive-Medical-Food
I would appreciate your input! Thanks a lot in advance.
Tags
carbon fiber
epoxy resin
food safe
high temp
tube
Edited
10 Years Ago by
valzine
Reply
Like
7
Replies
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Well you could fill with a cheaper resin, drill it out slightly larger than needed, then fill again with the food safe resin. Very labour wasteful though.
In all honesty, I don't think it would take a hell of a lot of resin to fill a tube of the pictured size. Probably 20ml or so, if that.
Reply
Like
8
valzine
valzine
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 6,
Visits: 21
Hanaldo (28/09/2016)
Well you could fill with a cheaper resin, drill it out slightly larger than needed, then fill again with the food safe resin. Very labour wasteful though.
In all honesty, I don't think it would take a hell of a lot of resin to fill a tube of the pictured size. Probably 20ml or so, if that.
Hanaldo, thanks a ton for your reply. What if I just use some kind of a foam applicator and paint it inside with a thick layer? Then drill to size? Would it work or the resin would just deform while being cured? Thanks!
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cover 10mm carbon fiber tube inside evenly with epoxy resin?
valzine
-
10 Years Ago
Why not cap one end,fill with resin when hard drill out and ream to size ?
f1rob
-
10 Years Ago
f1rob, thank you so much for your reply. That sounds like a good idea. Wouldn't that be wasting a...
valzine
-
10 Years Ago
Well you could fill with a cheaper resin, drill it out slightly larger than needed, then fill again...
Hanaldo
-
10 Years Ago
[quote][b]Hanaldo (28/09/2016)[/b][hr]Well you could fill with a cheaper resin, drill it out...
valzine
-
10 Years Ago
It just isn't very precise. The most precise way would be to completely fill them and then drill...
Hanaldo
-
10 Years Ago
Really the most precise way would be to make it in stainless wouldn't it ??? why has it got to be...
f1rob
-
10 Years Ago
[quote][b]f1rob (28/09/2016)[/b][hr]Really the most precise way would be to make it in stainless...
valzine
-
10 Years Ago
What sort of service temperatures and why must the inner aperture be 1/100th mm accurate? (how you...
ChrisR
-
10 Years Ago
[quote][b]ChrisR (29/09/2016)[/b][hr]What sort of service temperatures and why must the inner...
valzine
-
10 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search