			            bike frames commonly use UD for most of the construction, carbon does not like compression at all what spec of CF are you using in the tubes? The use of bonding metallic parts into the tube is how most frames are constructed but you need to ensure the surfaces are properly abraded and cleaned to get a good bond.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |