Hollow Boot Spoiler


Author
Message
Shane1985
Shane1985
Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)Supreme Being (192 reputation)
Group: Forum Members
Posts: 18, Visits: 175
Hi guys,

Planning for my first project / business Idea so please and yes I know it will be difficult so please don't shoot me down.

I want to make a CF version of the boot spoiler as pictured below, its hollow and probably about 2-3mm thick.

My question is: is there a way to make a 1 piece mold and then use the resin infusion to make the part?

Or

Does is have to be a split mold using prepreg (or resin infusion?)

Thanks guys

If the pics dont work please see Here


Shane
-Carbon Amateur-
*Never give up!*
Attachments
34pics239.jpg (1.2K views, 162.00 KB)
34pics241.jpg (907 views, 162.00 KB)
Edited 10 Years Ago by Shane1985
Reply
kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
im no expect, but going to say that should be done in a 2 piece mold