Group: Forum Members
Posts: 5,
Visits: 14
|
It happened in both cases.
the picture of the bigger pull up is when i was sanding an edge. the smaller ones is when i was cutting it.
Drilled some holes and same thing, big time delamination. It didnt bond nearly at all, i can basically peal it off.
not only i am unhappy about not making my deadline, but also i made a 8ft x 4ft sheet, so that is a huge cost in material i have to throw away.
|