just wanted to ask what clearcoat people are using? as in type and brand please

ive tried a few different types but never really been happy with them even with a flow coat 
Reply
Pugsport
Pugsport
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 14, Visits: 167
Hanaldo (22/05/2016)
No, acrylic and enamels are 1k paints. They work OK for clear coating, but their durability and chemical resistance are non existent. 2k coatings are a resin and a hardener, generally polyurethanes. 


2K is not a paint type but refers to the fact that he paint system is a 2 part system ie needing a hardener to make the paint go off. 

yes Acrylic and Enamel paints are 1k paint and dry throw solvent evaporation but its Acrylic Enamel which is a two paint and most people in the car restoration industry dont like it as they say it looks plastic .

im not 100% sure but i thought Polyurethane paints were mainly primers. where as Acrylic Enamel paints were primer, direct gloss topcoats and clear coats    
Edited 9 Years Ago by Pugsport
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search