Have anyone tried to made epoxy putty? There is so many ways to do it.. using aluminium powder, to get it transfer better the heat. using fiber glass, or glass bubbles.. I would be interested to hear how u have made it, and did it succeed? 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Ive made a bmc style compound by cutting up prepreg into 10mm lengths and smaller to do repair style pastes on aircraft.
The epoxy putty you can buy from ec is good for making tools but havent tried it for anything else.
What are you using it for? If its for a structural bmc material like quantum composites use for lamborghini wishbones i would buy direct from them.