I looking for post cure options. I want to make parts as large as a car hood, but I dont want to build a big oven. 

I have looked at these silicon heat blankets on ebay: 
http://stores.ebay.com/Flexible-Heaters/Silicone-Heater-Blankets-/_i.html?_fsub=10754115018&_sid=814680028&_trksid=p4634.c0.m322

http://thumbs3.ebaystatic.com/m/m5wq1sFhdbmdMXStPd9Nh2g/140.jpg


They are probably way to powerful so I may have to find some one that is not that powerfull per sqare cm. 

Iam thinking i can put some of these under the mold and wrap the mold with the heating elements with wool blankets. Then meassuring the temperature and control the heating to get the right temperature. Maybe using a PID or a temperature switch. 

Any thoughts?
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
That's how a lot of pre-preg boat hulls and aeroplane bodies are cured, so they do work. Quite a bit more involved than an oven though I think. 