Split mould leaking
Split mould leaking
Post Reply
Like
3
Split mould leaking
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Finnluxury
Finnluxury
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 50,
Visits: 448
Hi!
I would want some new ideas for a split mould. My last mould was leaking between the flanges. I am going to use resin infusion, so its critical that there is no air leaking. I included a photo of the part. It will be a three part mould. I will make splits above the door. Second photo has one idea I got, that the flanges would have 90 degree angle at the end, so i could put vacuum tape on it. blue and white line are different part of the mould. black line is plug. Top of the blue and white line is the vacuum tape.
Its impossible to vacuum bag the whole part, as its so huge. And I really wouldn't want to hand laminate this.
Reply
Like
3
Reply
VVS
VVS
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
If you put some break points in the flanges you will have no problem splitting it after.
don't know how clear this shows one but build if using wax same as you make location pegs from wax.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Split mould leaking
Finnluxury
-
9 Years Ago
Silicone liquid gasket is the easiest. The only issue is that it tends to 'bond' a little bit to the...
Hanaldo
-
9 Years Ago
[quote][b]Hanaldo (16/04/2016)[/b][hr]Silicone liquid gasket is the easiest. The only issue is that...
Finnluxury
-
9 Years Ago
Ive just done a 4 part mould and being much smaller but complicated used the silicon to seal . To...
VVS
-
9 Years Ago
Ok so different process using a sealed mould but you can see how they make the mould with wax and a...
VVS
-
9 Years Ago
Have attached a photo of my split mould channel. The channel is essential to the accuracy of the...
Hanaldo
-
9 Years Ago
If you put some break points in the flanges you will have no problem splitting it after....
VVS
-
9 Years Ago
I will test this silicon today. I bought Loctite SI 5926 blue as u menthioned. Thanks everyone for a...
Finnluxury
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search