Hi guys!

My friend is building 400+ HP Alfa 156 and wants carbon fibre bonnet, but in Czech republic is impossible to find larger carbon fabric than 1,2m wide and that's not enough.
So I want to ask you. What's the best way to made some big parts? Is it possible to connect 2 fabrics together in a center of part with some good looking finish? Or It's better to buy wider fabric and pay a lot of money for shipping from UK to Czech republic? That car is really low budget (car,engine and upgrades are less than 3000 gbp) and the prize is very important, but I want to make parts good looking too.

Thanks for your replies

-------------------Amateur from one little garage ----------Sorry for my English ----------------------------------------------
Edited 9 Years Ago by Pustil
Reply
VVS
VVS
VVS
posted 9 Years Ago HOT
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Ive looked at using some of the medical type tapes,

you can get some very thin fiber types that are porous.