Repairs to Carbon/Kevlar kayak or canoe


Author
Message
kayaker123
kayaker123
Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)Forum Member (42 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Hi 
Please could you recommend a product for 

1. general patching of carbon or carbon/kevlar kayaks
2. applying a new gel coat to carbon or carbon/kevlar kayaks

I've been told that for a tough gel coat you can mix a polyester resin with a polyester gel coat 50/50  - is this something you would recommend?  If so, is it the same hardener used for gel coat and resin?

thanks
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Jez,

If spraying's not an option and it's for the ongoing protection of the boat rather than bringing it up to a full glossy appearance then I think painting epoxy on would be a good way to go. Epoxy will bond better to whatever it is that the boat is made from than polyester would and if it's on the underside then we don't need to be particularly worried about UV protection so I'd suggest our Epoxy Coating Resin. You'll need to key-up the surface first (like we do in the video) and then your two options for the finishing of it would be to either pulling a release film tight over it or flatting and polishing it afterwards.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search