Just having a little trouble perfecting my resin infusion only my second attempt. can anyone help I think its degassing related but not 100% I have tiny gaps in the resin around the fibres only on the mould finish side none on the peel ply side. I assume this is air. Any ideas?? 
http://www.talkcomposites.com/Uploads/Images/49bda8d3-032c-4978-bb6f-7698.jpg
http://www.talkcomposites.com/Uploads/Images/42290ca4-912a-4c8b-84d2-c733.jpg
Dave
Edited 9 Years Ago by Davidpetty1988
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search