While ago i was looking for some small cf project just to practise more and i came up with this idea, make cf avalanche snow shovel for myself. At the beginning it was easy project, made 2 prototypes testing different fabrics, both came out very strong, just some pinholes. After testing them with snow and icy snow i realised that the tip of the shovel is not strong enough it crushed and they layers started to come apart little bit. Now im looking options what can i do to make the tip stronger, i was thinking some small metal insert to the tip, but havent figured out how to put it there. im happy to hear suggestions or other ideas how could i make it strong enough for icy snow.
 I used wetlayup and vacuum bag, after it was cured in oven i just trimmed the edges. 
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
You could make a narrow (2- 4 cm . ) strip of thin stainless steel and add at the edge as a layer in between the CF layers .. score/rough up the surface of the steel to make it bond properly to the CF/Epoxy ..

When you trim that edge -- sharpen it so that the steel edge sticks out a few mm ---  (I've made knives this way .. Cool ) Also make the "business edge of the shovel a bit thicker/stronger than the rest of the blade .. that's where you need the strength! Smile

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
We've been discussing this a bit recently as one of the other issues we see is the size of the shovel - it makes for a much larger back pack than you would otherwise need - poles, probes and the handle are relatively narrow once collapsed so it would be useful if the shovel itself could collapse or fold inwards so that you could use a camelback size backpack rather than a much larger one simply to accomodate the shovel itself.
taikuri
taikuri
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 13, Visits: 167
It will collapse, i have made one full carbon shovel already, which goes into 3 pieces like most this kind of shovels. 
its just the tip that has been the issue, so far. 
kidpaint
kidpaint
Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)Supreme Being (778 reputation)
Group: Forum Members
Posts: 99, Visits: 676
Idk if this will work but i have a plastic shovel with an aluminum strip riveted on. 
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Hi taikuri, I don't just mean that the handle will separate or fold from the shovel; I mean that the actual shovel blade itself (the digging part) will fold to make it much smaller; as well as having the detatchable or folding handle.

I've not seen one with a folding blade as well which I think would potentially be an awesome idea to make it really narrow and compact when stowed in a back pack.
taikuri
taikuri
Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)Supreme Being (111 reputation)
Group: Forum Members
Posts: 13, Visits: 167
Hi Richie.

Now i see what you mean, that would be great idea, but also can be difficult to make with the resources what i have in use. Im happy to hear ideas how that could be done.