I almost exclusively use the EC Epoxy Putty "system" for small moulds .. depending on the complexity of the shapes --
Some moulds I have made as a combination .. "green stuff" tooling Gelcoat, then even out details with the putty, then reinforce with glass-fibre or CF cut-offs as a strong backing
The Unimould system really depends on using chopped strand GF, but it works fine with finer glass-mats or woven --
If you want to use Pre-Preg .. go for the Unimould ..