posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
Have some weight bearing aerofoil shaped supports to make, which will have metal milled inserts bonded in for the hardpoints at each end. I can 3D mill the foam core, has anyone tried carbon skinning in an application that requires some strength? Would I be best doing it under a vacuum? Could I infuse? How would I ensure a cosmetic finish (I guess at the very least it'll need flatting back plus lacquer)
Any experiences/tips would be great to hear!
Edited
9 Years Ago by
jamesw
Reply
Like
3
Reply
jamesw
jamesw
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 558
The shrink tape is a good call!
I guess the "correct" method is a split mould, but it'll probably need to be pre-preg to lay it up given the dimensions... Two moulds and bonding the parts I guess should be strong enough?
James
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Structural Carbon over foam skinning
jamesw
-
9 Years Ago
You will need to get some sort of consolidation onto the fabric, but I've always found vacuum...
Hanaldo
-
9 Years Ago
The shrink tape is a good call! I guess the "correct" method is a split mould, but it'll probably...
jamesw
-
9 Years Ago
Again, depends on the dimensions. I infuse 4" internal diameter intake pipes in one shot, though...
Hanaldo
-
9 Years Ago
Where's f1rob when you need him! You haven't mentioned how big the part is so any advice will be...
ChrisR
-
9 Years Ago
I have made quite a lot of foils for boats using all sorts of techniques. If this part is loaded...
Fasta
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search