To ensure sufficient strength in an application like this, the only real option is to CNC mill a metal mould that can be heated and put under high pressure..
You can then use prepreg or hand lay up and expell the excess resin with the high pressure .  Your mould will have to be made with precision milled "channels" small enough to let the resin escape, but not allow fibres to block them.
I have tried to build this sort of thing for various parts for motorbikes and for firearms-stocks ..   It is extremely difficult to get a consistent, strong enough product .. 
IMHO it is not worth the effort for "one-offs" - 
 Also in this particular place you do not want the part to break/crack splinter, so you need at least some Kevlar/twaron/zytel in there .. 
A friend of mine simply took the complete saddle - pin assembly off the bike when correctly adjusted, and built a fixed position "carbon copy" of that ..
That way you can build it using the immense strength to weight ratio of a compound curved hollow carbon fibre part --   
This thing is less than a third of the combined weight of the original!!!  But also hard as a rock to sit on .. 
                
			            				
			            "Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)