I have made smaller moulds with the epoxy tooling gelcoat and epoxy putty. I have experienced that its easyest to put the hole mould in a bag and then do the infusion. 

But my question is what you do to complete the mould, do you put anything on the back of the mould to ensure that there is no sharpe dges to puncture the vacuum bag?
Reply
Ronny
Ronny
Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)Supreme Being (386 reputation)
Group: Forum Members
Posts: 58, Visits: 401
Listen to Hanaldo Wink
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search