Hi,

I'm looking to make a set of Carbon Fibre wishbones using tubes with aluminium bonded inserts.

Does anyone have any advice when it comes to bonding the aluminium to the carbon fibre to prevent pull out under high loads?

Specifically I am looking for advice on which glue to use and how to prepare the surface.

Thanks,

Dave
Reply
VVS
VVS
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
I cannot give advice on glue but I'd think any effect similar a knurled finish would be good,

I use to make stainless nut inserts for epoxy valves and we always knurled the outside.