Hi, I was wondering if anybody knows if the water clear resin would be any good for making micarta. I am after making it specifically for knife handles,and have seen that there are at least 2 different kinds,so did not know which would be best, or if either would be any good.
Thanks in advance !
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I use "infusion Polyester resin" from EC --- it is by far the best I've tried yet, and not nearly as expensive as Epoxy or Polyurethane -
The EC "Water cleat polyester casting resin" has too high a viscosity in my opinion, and does not work well when making cloth type micartas.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
satan
satan
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Brilliant, thankyou very much for your help !!