Hello, I was looking for Bi-axail and uni-directional cloth as the seem to be teh best strength/weight, and found suppliers that offers TRI and QUAD axial weaves. I know the fabric would get stiffer/ less drapable with every additional layer, harder to work with on curved surface. I was wondering, has anybody used a Tri/quad axail cloth before? Thought it might be an option for something like a pickup tonneau cover? What was your experience, Pros/Cons? The weaves look pretty trick/crazy, might be a nice option on style/looks?
1. http://www.directindustry.com/prod/formax/product-50648-546185.html[br]
2.http://www.multiaxialfabricselcom.com/en/Products/quadriaxial-fabrics-0o-45o-90o-45o.html[br]
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I often work with 600 and 850 GSM tri/quadaxials. They are a bit stiffer, but they aren't that bad. 

3600gsm is ridiculous though, that's serious stuff. Must be as stiff as a sheet of ali! 