Multi Axial cloth?


Author
Message
speed_demon
speed_demon
Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)
Group: Forum Members
Posts: 23, Visits: 163
Hello, I was looking for Bi-axail and uni-directional cloth as the seem to be teh best strength/weight, and found suppliers that offers TRI and QUAD axial weaves. I know the fabric would get stiffer/ less drapable with every additional layer, harder to work with on curved surface. I was wondering, has anybody used a Tri/quad axail cloth before? Thought it might be an option for something like a pickup tonneau cover? What was your experience, Pros/Cons? The weaves look pretty trick/crazy, might be a nice option on style/looks?
1. http://www.directindustry.com/prod/formax/product-50648-546185.html[br]
2.http://www.multiaxialfabricselcom.com/en/Products/quadriaxial-fabrics-0o-45o-90o-45o.html[br]
nc42
nc42
Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)
Group: Forum Members
Posts: 23, Visits: 365
haven't use it but would love to find someone who sells cut yardage of this: https://gernitex.com/product/spread-tow-carbon-fiber-fabric/
speed_demon
speed_demon
Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)Supreme Being (385 reputation)
Group: Forum Members
Posts: 23, Visits: 163
Yeah, I definitely like the 3D lookBigGrin plus those cloths are light(40-90gsm) so I could see using them like a surfacing veil over regular 2x2 twill. The ones I found were heavy,
#1. 400gsm all the way upto 1600gsm!
#2. offers quadaxial cloth 200-3600gsm! thats some thick stuff.
#3. tri axial was 532gsm the other was
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
If only easycomposites sold the Dense triaxial weave spread tow carbon fiber fabric Cool







David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 11 Years Ago by davro
nc42
nc42
Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)
Group: Forum Members
Posts: 23, Visits: 365
yeah, I'd love some of that in 240gsm. That said the price listed on the manufacturers website: 89 euros/m2!!!!
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Some of those are very nice looking fabrics!  As eluded to above, multiple layers and thicker fabrics can be harder to lay up as well as wet out in some circumstances.  Other than the unique cosmetic appeal, the structural reasons for such clothes would generally be fairly specific.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I often work with 600 and 850 GSM tri/quadaxials. They are a bit stiffer, but they aren't that bad. 

3600gsm is ridiculous though, that's serious stuff. Must be as stiff as a sheet of ali! 
nc42
nc42
Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)Supreme Being (275 reputation)
Group: Forum Members
Posts: 23, Visits: 365
one nice thing with the 0/+-60 spread tow is that it makes for quasi-isotropic plys which would be nice for single skin panels