or, now that you have made the CF part nice and smooth on the outside, just wax it very carefully place it on the plug and make a new "female" mould on top of it..
Then you have a mould of both sides of the piece, and you can use the plug for compressing the wet layup in the new mould . (I'm assuming you did this as a wet-lay without vacuum?)
If you have a vac kit/setup then just do a wet-lay and vac-bag in the new female mould..