Pin holes appearing using GC50
Pin holes appearing using GC50
Post Reply
Like
2
Pin holes appearing using GC50
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
MarkMK
MarkMK
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 338,
Visits: 2K
Hi All
A couple of recent parts have come out with pin holes all over. Both received a good coat of GC50 sprayed before infusion under full (and drop tested) vacuum.
Clearly there's very little time to allow the coating to de-gas prior to spraying, so wondering if it might be an issue with the gun/compressor causing this?
Anyone experienced similar?
Thanks
Reply
Like
2
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Can you post photos?
Reply
Like
3
MarkMK
MarkMK
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 338,
Visits: 2K
It won't let me add pics direct, so I've posted a link to one I've just taken. Not easy to get a decent shot on the curved surface, but hopefully you'll see enough.
https://www.dropbox.com/sc/xcnvm2s76i55stm/AADevknoAgaM9O2JbENvSGWBa
If you zoom in the surface looks horrendous, but perhaps the crater-like appearance is just normal and we don't usually zoom in that much, but the little holes are concerning.
I sprayed another couple of parts at the same time as this one and haven't experienced the same issue with those, so a bit baffling. I believe I laid down the coat pretty consistently and it was left overnight before layup the next day. From a few feet away all looks nice and glossy, but didn't expect this from an in-mould coating. No humidity or cold issues that I can think of either.
I did use a small amount of Aerofix3 to help position, but all I've seen previously is the occasional dull spot from this where I might have not misted the spray quite carefully enough.
Not the easiest thing to do with the cup gun, but I will try to do a gentle mist coat first and leave for a couple of minutes before adding more, to see if that helps eliminate this
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search