Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Film adhesive for honeycombe core materials
Film adhesive for honeycombe core materials
Post Reply
Like
3
Film adhesive for honeycombe core materials
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Toffee
Toffee
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 36,
Visits: 118
Hi all,
I am making sandwich panel and i am looking at making the carbon skins first and then sticking each layer to either side of a nomes honeycomb core material. I have thought of four options here >
1. make the outer skins, key the back of them paint brush resin on to the skins and stick either side of the honeycomb, then vacuum
2. make the outer skins, key the back of them soak the honeycomb in resin and stick either side of the honeycomb, then vacuum
3. make the outer skins, key the back of them adda 400g pre-preg layer to the back of the skins and stick to the core, vacuum, oven…
4. same as options 1 & 2 but instead of using resin use a film adhesive, question is where can i get this from, is there different weights of adhesive if so which is most suitable and where do i get it from??
hope you can help,
Lee.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Film adhesive for honeycombe core materials
Toffee
-
10 Years Ago
The first option is perfectly adequate. Use peel ply when you're making the outer skins and you...
Hanaldo
-
10 Years Ago
Thats great feedback thanks very much, i am going to try options 1&2 on Saturday on two test pieces,...
Toffee
-
10 Years Ago
[quote][b]Toffee (29/07/2015)[/b][hr]Hi all, I am making sandwich panel and i am looking at making...
fgayford
-
10 Years Ago
Did a part using nomex just last week and had a play about before committing. I found brushing gave...
VVS
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search