Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
Sealing Foam Buck?
Sealing Foam Buck?
Post Reply
Like
3
Sealing Foam Buck?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Dave
Dave
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 48,
Visits: 253
Check this thread out:
http://www.talkcomposites.com/56/Foam-Pattern-to-a-Gloss-Finish
"
Sure. The ratios arn't too critical with either the bubbles or the silica and will really depend on the consitancy you want the 'pattern coat' to be. The more bubbles you add, the more sandable the coat will be but the less tough it will be. The more silica you add the thicker it will be (the bubbles will also make it thicker too). It's a case of adding until it seems about right. I would guess by weight only maybe 10% bubbles and a few percent silica. The thing to watch out for with the silica is that it takes a while to 'take effect' on the resin because the crystals take time to absorb the resin (several hours to reach full properties) and also a decent amount of agitation so my suggestion would be to add a few percent by weight to the resin (with no hardener added) first and let them soak in the resin for a few hours before giving it a really good stir. You'll be able to guage how thixotropic it then is and then add your bubbles and hardener once you're happy."
Dave.
Reply
Like
3
neilb
neilb
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 107,
Visits: 504
i'm guessing you want to make the epoxy resin more thixotropic?
Reply
Like
2
jamesw
jamesw
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
Can anyone suggest a good mix ratio for a foam pattern sealer?
I understand I need
Epoxy Coating Resin
Glass bubbles
Silica
Could do with some graphite to give a black colour
Many Thanks,
James
Edited
13 Years Ago by
jamesw
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search