I do not seem to have all that much of a problem with the "Gel Coat Cup Gun" from EC ... The real trich is to run it at a lower pressure than a "normal" compressor delivers.. I bought a reduction valve from my local supplier, an have set that to 4 bar (= 58 psi) That makes the "cup Gun" much easier to use. But the dripping is something that you will have to live with.
Generally I only spray outside under an open roof. I really do not want styrene based droplets all over my workshop .. This of course means only spraying in nice weather ... Since I'm not trying to make a living out of this, it's not really a problem.