Hi mate nice job,did you get my pm the other week re work/Bristol ? Was messaging someone the other day and cant see the message I sent you in any of my folders ?
re the mirrors any wet lay I do I cut a square of material big enough to cut all my templates out,lay that on a sheet of plastic,pour my resin on and use a squeegee or filler spreader to move the resin around and wet out the cloth
Another sheet of plastic on top then you can mark your template shape out on the plastic an cut out with scissors
LOT easier than wetting out individual templates
Also sometimes you can get better results with a bleed on the job rather than pulling full vac
P.S you can do that in preepreg !!!
Use one of your wetlay mirrors as a former,heat an drape your prepreg over it,quick 10 minute chill in the freezer then pop it off an drop it in the Ali
|