I have put 2 coats of coating epoxy onto marine ply.
Then I applied one coat of Epifanes varnish 48 hours ago. The varnish is not drying.
Is there an incompatibility?
Should I wash the epoxy coating, as I have read elsewhere?
One professional adds cobalt drier to the varnish to fix the problem. Do you know about this?
I have only used a test piece of plywood so far. Also a narrow strip of pine (same problem).
Thanks
|