Yes the formulation changed meaning acetone does not activate it in the same way as before. Acetone could well end up attacking any area that is not fully cured which would make things worse if you have holes in the gelcoat when it comes to infusion.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|