Hi,

I am trying to make a stool with braided carbon sleeve 20mm. I am wondering how sturdy it is with epoxy resin. Is it durable enough not to snap bearing the body weight like links attached below? Otherwise, could you give me any advice to make it harder as a seat?

Here is links as an example. 

http://www.dailytonic.com/carbon-fibre-seats-by-peter-donders-be/
http://www.artnet.com/Artists/LotDetailPage.aspx?lot_id=9C9BAD102F4BAE377573FE6B1429EC8B

Thanks for your help.
Replies
yooou
yooou
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 3, Visits: 52
Hi Matthieu,

Thanks for your advice! It is a nice lovely chair. I will apply one layer of carbon fabric at first and see
how more layers I would need.



yooou
yooou
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 3, Visits: 52
Hi Matt,

Thanks for your opinion. I got a few more question.

I have ordered 5m of cf sleeve and IN2 resin for testing. How can I apply resin to the sleeve? Using brush? Dipping?or Spray?

To get a nice finishing, what should I do with the surface of sleeve after it cures? As you said, would a spray gun make the surface smooth?

Thanks for your help.
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)Composites Expert (Staff) (8.5K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Yooou,

How can I apply resin to the sleeve? Using brush? Dipping?or Spray?


I would suggest that brush application would probably still be best. Dipping might work, providing that you agitate the braid enough whilst it is in the resin, so that the resin can wet the fibres thoroughly. Spraying would probably not allow the fibres to wet-out properly so I would avoid it.

To get a nice finishing, what should I do with the surface of sleeve after it cures? As you said, would a spray gun make the surface smooth?


It depends what sort of a finish you want. If you want a smooth, glossy finish then it might be worth wrapping the sections with release film or shrink tape whilst they are still wet to make them less textured once they are cured. After this, you could flat them back and then either lacquer (clear coat) them or paint a layer of epoxy coating resin on them, before flatting and polishing that.

If you actually want a textured finish then you could just leave it in its natural state or spray lacquer onto the braid and leave it.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search