I would like to cover the Kitchen Worktop, in my camper with a single layer of carbon cloth and hi temp laminating reason.

I was intending to use

Carbon Fibre 2/2 Twill 3k 199g

Very High Temperature Epoxy Laminating Resin 500g Pack

I have done a few structural repairs with carbon before but that is it, so I understand how to lay the fibre and resin, but I am looking for advice or a guide on how to get a flat gloss finish, ideally a mirror like one.
Reply
surferx
surferx
Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)Supreme Being (81 reputation)
Group: Forum Members
Posts: 8, Visits: 60
Need a bit of help/advice on how to proceed...

Laid the carbon down with the excess resin, the carbon is down nicely etc. But as I ran out of time... I rushed the last coat of resin, and I could not get hold of polypropylene or glass sheet to put over it.

anyway...

I was thinking of flatting it back using my sander 400 through to 2000 and polish etc as recommend in this thread.

But I would ignore the worst of the low spots, sort of like a practise run...

Once I done my best put another thin coat of resin to fill the low spots and sand and polish again. That way I get a bit of practise... so when i do my final coat I have more idea of what I am doing...

Does this seem like a workable plan? what will I need to remove the polish compound if go down this route before I overcoat with resin?

I could get a polypropylene sheet, and do another layer of resin, though I am loathe to do this now, as I still may make a mistake. At least if I flat off and polish what I have now I will have a practise before I do the final coat.
Attachments
IMG_20150521_092331_730.jpg (519 views, 1.00 MB)
Edited 10 Years Ago by surferx